E-GLASS FIBER INSULATION /EXHAUST PIPE INSULATION /Pre-Slit Tubular E-glass Fiber Pipe Cover with AluglassJackets
Product |
E-glass insulation tube(alkali-free fiberglass insulation tube ) |
Inner diam: |
20~300mm |
Volume density: |
120~300kg/m³ |
Max temp for 3 different models respectively |
1.650ºC(1202°F), 2.800ºC(1472°F), 3.1000ºC(1832°F) |
Max temp. |
1000ºC(1832°F) |
Long term temp. |
550ºC (932°F) |
Features |
Low price, fireproof, flame retardant, and high temperature resistant |
Descriptions:The molded pipes (circular/irregular) made from e-glass wool felt using inorganic adhesive.
Advantages:it possesses excellent thermal insulation, sound absorption, corrosion resistance, electric insulation, and high temperature resistance. It is easy to assemble and disassemble reducing much labour cost and time.
Usage: Widely used as insulating tube for motorcycle and automobile exhaust pipes, chemical pipelines, sewage pipelines, pipes in thermal power plants, and other high temperature pipes.
The e-glass insulation tubes or elbows available with different specifications and 3 different max temperatures.
E-glass Fiber Tube Temperature Classification & Physical Properties
A-1 Temperature 650ºC,A-2 Temperature 800ºC,A-3 Temperature1000ºC
Chart A-1 |
||
Type of glass |
E-glass fiber (650ºC) |
|
Glass composition |
Composition |
Accounted for (%) |
SiO2(Silicon dioxide) |
52~56 |
|
CaO(Calcium oxide) |
16~25 |
|
AL203(Alumina) |
12~16 |
|
B2O3(Boric anhydride) |
5~10 |
|
MgO(Magnesium oxide) |
0~5 |
|
Na2O+K2O(Alkali) |
0~2 |
|
Glass fiber diam |
9μ |
|
Glass fiber length |
≥50mm |
|
Density(Central value) |
100kg/m3 |
|
Chart A-2 |
||
Type of glass |
Heat resistant E-glass fiber (800ºC) |
|
Glass composition |
Composition |
Accounted for (%) |
SiO2(Silicon dioxide) |
54~62 |
|
CaO+ MgO(Calcim oxide+Magnesium oxide) |
17~26 |
|
AL203(Aluminu) |
12~16 |
|
B2O3(Boric anhydride) |
5~10 |
|
Na2O+K2O(Alkali) |
0~2 |
|
Glass fiber diam |
9μ |
|
Glass fiber length |
≥50mm |
|
Density(Central value) |
100kg/m3 |
|
Chart A-3 |
||
Type of glass |
High silica fiber(1000ºC) |
|
Glass composition |
Composition |
Accounted for (%) |
SiO2(Silica dioxide) |
90~95 |
|
AL203(Aluminu) |
2~6 |
|
CaO(Calcium oxide) |
- |
|
Na2O(Alkali) |
- |
|
other |
0~1 |
|
Glass fiber diam |
9μ |
|
Glass fiber length |
≥50mm |
|
Density(Central value) |
120kg/m3 |